Granularite ak anbalaj
Ferrotungstènese delivre nan fòm blòk oswa granulaire.
Anbalaj: 250kg tanbou fè, kapab tou apwovizyone selon kondisyon itilizatè.
Ferotungstèn komen gen ladan de klas: ferrotungstène 70 ak ferrotungstène 80. Akòz gwo pwen k ap fonn li yo, ferrotungstène souvan pwodui pa metòd aglomerasyon an oswa metòd ekstraksyon fè.
Kèk
Konpozisyon Ferrotungstèn
|
Klas |
Kèk 8OW-A |
Kèk80-B |
KEK 80-C |
|
W |
75%-80% |
75%-80% |
75%-80% |
|
C |
0.1% max |
0.3% max |
0.6% max |
|
P |
0.03% max |
0.04% max |
0.05% max |
|
S |
0.06% max |
0.07% max |
0.08% max |
|
Si |
0.5% max |
0.7% max |
0.7% max |
|
Mn |
0.25% max |
0.35% max |
0.5% max |
|
Sn |
0.06% max |
0.08% max |
0.1% max |
|
Cu |
0.1% max |
0.12% max |
0.15% max |
|
Kòm |
0.06% max |
0.08% max |
0.10% max |
|
Bi |
0.05% max |
0.05% max |
0.05% max |
|
Pb |
0.05% max |
0.05% max |
0.05% max |
|
Sb |
0.05% max |
0.05% max |
0.05% max |
|
Sn |
0.06% max |
0.08% max |
0.08% max |
Nou gade pou pi devan pou kolabore avèk ou, si ou gen nenpòt kesyon oswa bezwen sou pwodwi nou yo ak sèvis, tanpri ou lib pou kontakte nou:info@zaferroalloy.com.