1.Fil nwayoka ogmante sede alyaj, diminye depans fusion, diminye tan fusion, ak kontwole avèk presizyon engredyan.
2. Fil cored ka amelyore kalite asye fonn ak amelyore eta Distribisyon an.
3. Fil nwayo divize an de kalite: kalite entèn trase ak kalite ekstèn trase, ki okipe mwens espas epi yo fasil pou itilize.
Alyaj nwayo fil

Paramèt pwodwi
| Klas | Kontni | Fil Dyamèt (mm) |
Epesè senti asye (mm) |
pwa senti asye (g/m) |
Pwa poud |
Inifòmite (%) |
| Casi | Si55Ca30 | 13.0 | 0.4 ±0.05 | 145 | 230 | 2.5-5.0 |
| Kabinè | Ca26-30Al3-24 | 13.0 | 0.4 ±0.05 | 145 | 210 | 2.5-5.0 |
| KaFe | Ca28-35Fe | 13.0 | 0.4 ±0.05 | 145 | 240 | 2.5-5.0 |
| Kasiba | Si55Ca15Ba15 | 13.0 | 0.4 ±0.05 | 145 | 220 | 2.5-5.0 |
| Bazal | Si35-40Al12-16Ba9-15 | 13.0 | 0.4 ±0.05 | 145 | 215 | 2.5-5.0 |
| KaSiAl | Ca30-35Al7-8Si<0.8 | 13.0 | 0.4 ±0.05 | 145 | 200 | 2.5-5.0 |
| Kasiba | Si{{0}Ca{{1{1}} Ba6-12Al12-18 |
13.0 | 0.4 ±0.05 | 145 | 225 | 2.5-5.0 |
Zhenan gen plis pase 30 ane eksperyans nan travay nan jaden métallurgique e li te rive jwenn koperasyon alontèm ak 50,000+ kliyan atravè mond lan. Pwodwi yo li bay yo se nan bon jan kalite serye ak pite segondè. Si ou vle konnen pri a, tanpri kontakteinfo@zaferroalloy.com.