Silicon Carbide Black 53C. Grinding Grain F36

Silicon Carbide Black 53C. Grinding Grain F36

Black silicon carbide chips are formed at 2000 degree or higher, using silica sand and coke as material, after various chemical processes.
Voye rechèch
Dekri teren
Karakteristik teknik
Silicon carbide black 53C. Grinding grain F36 Description

 

Black silicon carbide grits are formed at 2000 degree or above, using silica sand and coke as material, after various chemical processes.

1.SIC has strong resistance to high temperature.
2.Silicon carbide has corrosion resistance.
3.Silicon carbide has wear resistance.
4.Strong thermal and electrical conductivity.

product-600-500

 

The Specification Of Silicon carbide black 53C. Grinding grain F36

 

1-3mm,3-5mm,16,24,30,36,46,60,100,120,150,200,280,325,1000 mesh

Greater than or equal to 97%

Greater than or equal to 90%

2O3 Content

Less than or equal to 1.2%

Less than or equal to 1.5%

F.C

Less than or equal to 0.3%

Less than or equal to 0.5%

3.2g/cm3

2730 degree

2840-3320kg/mm2

9.0

 

Packed in 25kg/bag(PP/PE) or 1 MT jumbo bag,or as per the requirements of clients

 

 

F36 Black Sic Silicon Carbide Grit for saleF36 Black Sic Silicon Carbide Grit price

 

 

 