Ferrochromium se yon alyaj fè ak chromium ak fè kòm eleman prensipal li yo. Li se youn nan ajan alyaj prensipal yo nan endistri asye a. Ferrochrome gen ant 50% ak 70% chromium.

 

fèwokòl

ferrochrome

Klasifikasyon Ferochrome

Klas Konpozisyon chimik (%)
Kr C sizo P S


Mikwo kabòn
FeCr-1 58-68 0.03-0.15 1.0-2.0 0.03-0.06 0.025-0.03
FeCr-2 63-68 0.03-0.15 1.0-2.0 0.03-0.06 0.025-0.03


Ba kabòn
FeCr-3 58-68 0.25-0.5 1.5-3.0 0.03-0.06 0.025-0.03
FeCr-4 63-68 0.25-0.5 1.5-3.0 0.03-0.06 0.025-0.03


Mwayen kabòn
FeCr-5 58-68 1.0-4.0 1.5-3.0 0.03-0.06 0.025-0.03
FeCr-6 63-68 1.0-4.0 1.5-3.0 0.03-0.06 0.025-0.03


Segondè kabòn
FeCr-7 58-68 4.0-10.0 3.0-5.0 0.03-0.06 0.03-0.06
FeCr-8 63-68 4.0-10.0 3.0-5.0 0.03-0.06 0.03-0.06

 

Zhen'an Metallurgy se yon founisè pwofesyonèl pwodwi métallurgique nan Lachin ak bon jan kalite segondè, pri konpetitif ak gwo repitasyon. Byenveni nan vizite faktori nou an.