Ferrosilicon 75 paramèt ki gen rapò

Apr 12, 2024 Kite yon mesaj

Abreviyasyon:fesi 75
Gwosè: 10-50mm, 50-100mm, yo ka Customized
Fòm: boul, poud, boul
Paramèt detaye: si pi gran pase oswa egal a 75
Itilizasyon: deoksidasyon, asye, Distribisyon, elatriye.

Ferosilicon 75

ferro silicon 75

Ferrosilicon 75 engredyan

Modèl Konpozisyon chimik (%)
sizo Mn al C P S
Fesi75a 75.0-80.0 Mwens pase oswa egal a 0.4 Mwens pase oswa egal a 2.0 Mwens pase oswa egal a 0.2 Mwens pase oswa egal a 0.035 Mwens pase oswa egal a 0.02
Fesi75b 73.0-80.0 Mwens pase oswa egal a 0.4 Mwens pase oswa egal a 2.0 Mwens pase oswa egal a 0.2 Mwens pase oswa egal a 0.04 Mwens pase oswa egal a 0.02
Fesi75c 72.0-75.0 Mwens pase oswa egal a 0.5 Mwens pase oswa egal a 2.0 Mwens pase oswa egal a 0.1 Mwens pase oswa egal a 0.04 Mwens pase oswa egal a 0.02

 

Nou se yon mak inik nan mache a ki ofri yon seri eksklizif nan pwodwi métallurgique pou kliyan valè nou yo.