A pwezan, pwensipal ekipman pou anwo nan syèl la Titàn fèt an fè nan mache entènasyonal la se w (Ti) 68 meyè kalite anwo nan syèl la Titàn fèt an fè ak 72%, w (Al)<4.0%, w (Si)<0.5%, w (N)<0.4%, w (C)<0.1%, w (S)<0.015%, w (P)<0.02%, and w (TO)<1.0% is produced using the titanium chip remelting method. This method is also used domestically to produce high titanium iron, but the cost is high.
In order to reduce steelmaking costs, domestic steel companies have appropriately lowered their requirements when purchasing high titanium iron. The requirements for high titanium iron used in the production of IF steel by W plant are: w (Ti)>65%, w (Al)<4.5%, w (Si)<0.5%, w (TO) 65%, w (Al)<4.0%, w (Si)<0.5%, and w (TO)<5.0%.