Ferosilicon 75 boul Deskripsyon
Ferosilicon 75 vle di Si pi gran pase oswa egal a 75% C mwens pase oswa egal a 0.2% S mwens pase oswa egal a 0.02% P mwens pase oswa egal a {{10}}.04% Al Mwens pase oswa egal a 1.5% Cr Mwens pase oswa egal a 0.5% Mn Mwens pase oswa egal a 0.5% Ca Mwens pase oswa egal a 1%, Nou sitou bay 75 ferrosilicon, 72 ferrosilicon, 65 ferrosilicon, 45 ferrosilicon, asirans kalite ferrosilicon, livrezon alè, selon kondisyon kliyan an, bay blòk natirèl, blòk estanda, granules, poud, ak lòt pwosesis grenn jaden.
![]()
Spesifikasyon Ferrosilicon 75 boul
| C | sizo | Mn | S | P | Kr | al |
| jiska 0.1 | 74 - 80 | jiska 0.4 | jiska 0.02 | jiska 0.04 | jiska 0.3 | jiska 3 |
Gwosè:
1. boul: 10-30mm, 30-50mm, 50-100mm, oswa selon kondisyon kliyan an.
2. Briquette: 50 * 50mm oswa selon kondisyon kliyan an.
3. Poud: 325mesh, 200mesh, 300mesh, 65mesh oswa Customized.
4. Granules: 0.3-1mm, 1-3mm, 3-8mm oswa Customized.
Ferrosilicon 75 moso anbalaj:Adopte bon jan kalite tòn sak pou anbalaj asire sekirite nan transpòte machandiz, selon kondisyon kliyan, lè l sèvi avèk ankadreman an bwa oswa tanbou fè pou anbalaj, lè l sèvi avèk transpò tè ak lanmè, bon jan kalite ferrosilicon 75 pral transpòte nan tout pati nan mond lan.
![]()
![]()
FAQ
K: Ki tèm peman an?
A: kondisyon peman nou yo negosyab.
K: Mwen gen kèk kondisyon espesyal sou espesifikasyon yo.
A: Nou gen yon seri pwodwi byen awondi, ki ba nou kapasite pou aplike anpil espesifikasyon espesyal. Tanpri santi yo lib pou kontakte nou ak ou.
K: Èske ou aksepte sèvis OEM?
A: Wi, nou fè sa.
K: Ki sa ki sou dat livrezon ou a nan kondisyon nòmal?
A: Nou voye kago a nan 15 jou apre nou fin resevwa depo garanti a.
Baj popilè: ferrosilicon 75 boul, Lachin ferrosilicon 75 boul manifaktirè, Swèd