72 Ferrosilicon boul Deskripsyon
Silica for smelting 72 pieces of ferrosilicon requires SiO2>97% 25, Al2O3<1.0%, CaO<0.5%, P2O5<0.03%. Silica for smelting 72 pieces of ferrosilicon should not burst during the heating process. Before smelting 72 pieces of ferrosilicon, the silica should be washed to remove adhering soil and impurities.

72 FeSi Alloy Konpozisyon
| Modèl NO. |
| ferro silicon 72 |
| Sèvi ak |
| Asye |
| Kalite |
| Ferro Silisyòm alyaj |
| Pake transpò |
| 1mt gwo sak |
| Spesifikasyon |
| 1-3mm, 3-10mm, 10-50mm, 50-100mm oswa Customized |
| mak |
| Zhenan |
| Orijin |
| Lachin |
| Kapasite pwodiksyon |
| 2000 tòn/Mwa |
Kòm yon founisè nan 72 boul Silisyòm ferro pou 30 ane, faktori nou an kouvri yon zòn nan 30, 000 mèt kare e li gen 2 ansanm nan 6300KVA alyaj raffinage founo, 8 ansanm nan founo frekans mwayen, elatriye.
![]()
![]()
FAQ
K: Konbyen tan se tan an livrezon pou lòd esansyèl?
A: Sa depann de kantite lòd la, nòmalman tan livrezon an pral 7-15 jou travay. Tanpri tanpri kontakte nou anvan kòmande.
K: Èske sèvis OEM/ODM disponib?
A: Wi, nou aksepte OEM/ODM.
K: Si mwen bezwen anbalaj Customized, èske sa ki disponib?
A: Wi, nou ka bay espesifikasyon diferan nan sache oswa tanbou asye selon kondisyon ou yo.
K: Èske w se yon manifakti?
A: Nou se yon manifakti ak founisè ki gen plis pase 30 ane eksperyans nan Henan, Lachin.
Nou gen yon moun QC rete sou liy pwodiksyon yo akòz enspeksyon an. Tout pwodwi yo dwe te enspekte anvan livrezon. Nou fè yon enspeksyon inline ak yon enspeksyon final.
1. Tout matyè premyè yo tcheke yon fwa yo rive nan faktori nou an.
2. Tout moso ak logo ak tout detay tcheke pandan pwodiksyon an.
3. Tout detay anbalaj yo tcheke pandan pwodiksyon an.
4. Tout bon jan kalite pwodiksyon ak anbalaj tcheke sou enspeksyon final la apre fini.
Baj popilè: 72 ferro Silisyòm boul, Lachin 72 ferro Silisyòm boul manifaktirè, Swèd