Ferovanadiumse delivre nan blòk oswa fòm granulaire.
Gwosè: 03 - 20mm, 10 - 50mm
Anbalaj: tanbou asye (25kg, 50kg, 100kg, 250kg) oswa 1 tòn sak.
Remak: Konpozisyon chimik, gwosè patikil, ak anbalaj pwodwi ki anwo yo ka Customized selon bezwen kliyan yo.
fev

Paramèt Ferrovanadium
| Klas | V | al | P | sizo | C |
| FeV40-A | 38-45 | 1.5 | 0.09 | 2 | 0.6 |
| FeV{{0}B | 38-45 | 2 | 0.15 | 3 | 0.8 |
| FeV50-A | 48-55 | 1.5 | 0.07 | 2 | 0.4 |
| FeV{{0}B | 45-55 | 2 | 0.1 | 2.5 | 0.6 |
| FeV60-A | 58.0~65.0 | 1.5 | 0.06 | 2 | 0.4 |
| FeV{{0}B | 58.0~65.0 | 2 | 0.1 | 2.5 | 0.6 |
| FeV60-A | 58.0~65.0 | 0.4 | 2 | 0.06 | 0.04 |
| FeV{{0}B | 58.0~65.0 | 0.6 | 2.5 | 0.1 | 0.05 |
| FeV80-A | 78-82 | 1.5 | 0.05 | 1.5 | 0.15 |
| FeV{{0}B | 78-82 | 2 | 0.06 | 1.5 | 0.2 |